EN19T or EN24T? Choosing the Right Through-Hardening Alloy Bar
EN19T and EN24T are two of the most widely specified through-hardening alloy steels in UK engineering. Both are supplied hardened and tempered, both machine well in that condition, and both turn up on drawings for shafts, gears, spindles and high-stress components. So why do engineers and buyers so often ask which one to use? Here is how to choose, from the team at Midland Special Steels.
What they have in common
Both grades are medium-carbon alloy steels supplied in the “T” condition, which is hardened and tempered to a tensile strength range of around 850 to 1000 N/mm². In that condition they can be machined directly, with no heat treatment needed afterwards for many applications.
Where they differ
The difference is in the alloying elements.
- 708M40T (EN19T) is a chromium-molybdenum steel. It offers a good balance of strength, toughness and wear resistance, and is a dependable general-purpose choice for medium-stress components.
- 817M40T (EN24T) is a nickel-chromium-molybdenum steel. The addition of nickel improves toughness and hardenability, meaning it responds more fully to heat treatment, particularly in larger sections.
In practice, that makes EN24T the usual choice where a part is heavily loaded, subject to shock or fatigue, or has a larger cross-section.
How to choose
A few questions help narrow it down:
- How large is the section? Larger diameters are harder to harden right through. EN24T’s hardenability gives it an advantage as sizes increase.
- What loads will the part see? For shock, impact or high cyclic loading, the extra toughness of EN24T is often worth having.
- Is cost a driver? EN19T is generally the more economical option, so where its properties meet the requirement there is no need to specify more than the job needs.
- Will it be heat treated further? If you plan to harden to a higher strength after machining, check the grade and size suit your process and talk to your heat treater.
Do not forget certification
Whichever you choose, ask for material certification so that the grade, condition and heat number can be traced. Our post on material traceability explains why that matters.
Need a steer?
If you are unsure which grade suits your component, the Midland Special Steels team can help. Tell us the application, section size and the properties you need, and we will advise on the right bar from stock.